ASTM A131 Specification

PropertyDetails
StandardASTM A131
Grades AvailableA, B, D, E, AH32, DH32, EH32, AH36, DH36, EH36
DimensionsASTM A131 Grade A, B, D, and E
Thickness: 0.1875–3.94 in (4.762–100 mm)
Length: 240–1020 in (6100–25910 mm)
Width: 72–129.9 in (1800–3299 mm)
ASTM A131 Grade AH/DH 32
Thickness: 0.251–1.50 in (6.38–38.1 mm)
Length: 240–1020 in (6100–25910 mm)
Width: 72–120 in (1800–3050 mm)
ASTM A131 Grade AH/DH/EH 36
Thickness: 0.251–3.94 in (6.38–100 mm)
Length: 240–1020 in (6100–25910 mm)
Width: 72–129.9 in (1800–3299 mm)
Mechanical PropertiesYield Strength: 235 – 355 MPa, Tensile Strength: 400 – 620 MPa
Chemical CompositionCarbon, Manganese, Silicon, Phosphorus, Sulfur
FeaturesHigh strength, good toughness, corrosion resistance, weldability
ApplicationsShip hulls, decks, superstructures, offshore platforms, marine engineering
Category:

Description

ASTM A131 Shipbuilding Steel Plate

ASTM A131 is the standard specification for structural steel used in shipbuilding. It covers different grades of carbon and high-strength low-alloy (HSLA) steel plates, primarily designed for use in the construction of ships and offshore structures.

Key Grades of ASTM A131 Steel

  • Grade A, B, D, and E – Carbon steel plates with varying mechanical properties.
  • Grade AH32, DH32, EH32, FH32 – High-strength grades with a minimum yield strength of 315 MPa.
  • Grade AH36, DH36, EH36, FH36 – High-strength grades with a minimum yield strength of 355 MPa.
  • Grade AH40, DH40, EH40, FH40 – High-strength grades with a minimum yield strength of 390 MPa.

Dimensions

ASTM A131 Grade A, B, D, and E

  • Thickness: 0.1875–3.94 in (4.762–100 mm)
  • Length: 240–1020 in (6100–25910 mm)
  • Width: 72–129.9 in (1800–3299 mm)

ASTM A131 Grade AH/DH 32

  • Thickness: 0.251–1.50 in (6.38–38.1 mm)
  • Length: 240–1020 in (6100–25910 mm)
  • Width: 72–120 in (1800–3050 mm)

ASTM A131 Grade AH/DH/EH 36

  • Thickness: 0.251–3.94 in (6.38–100 mm)
  • Length: 240–1020 in (6100–25910 mm)
  • Width: 72–129.9 in (1800–3299 mm)

ASTM A131 Chemical Composition

Element A/B/D/E (%) AH32/DH32/EH32 (%) AH36/DH36/EH36 (%)
Carbon (C) 0.21 max 0.18 max 0.18 max
Manganese (Mn) 2.5 × C min 0.90 – 1.60 0.90 – 1.60
Phosphorus (P) 0.035 max 0.035 max 0.035 max
Sulfur (S) 0.035 max 0.035 max 0.035 max
Silicon (Si) 0.10 – 0.35 0.10 – 0.50 0.10 – 0.50

ASTM A131 Mechanical Properties

Grade Yield Strength (MPa) Tensile Strength (MPa) Elongation (%)
A 235 min 400 – 520 22 min
B 235 min 400 – 520 22 min
D 235 min 400 – 520 22 min
E 235 min 400 – 520 22 min
AH32 315 min 440 – 590 22 min
DH32 315 min 440 – 590 22 min
EH32 315 min 440 – 590 22 min
AH36 355 min 490 – 620 21 min
DH36 355 min 490 – 620 21 min
EH36 355 min 490 – 620 21 min

Applications

  • Ship hulls and decks
  • Offshore platforms
  • Marine structures
  • Oil rigs and ship repairs

Reviews

There are no reviews yet.

Be the first to review “ASTM A131 AH36, DH36, EH36, FH36 Shipbuilding Steel Plate”

Your email address will not be published. Required fields are marked *


The reCAPTCHA verification period has expired. Please reload the page.